Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fainplast Compounds RKI 0223 Rigid PVC, Antishock Injection Molding Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds RKI 0223 Rigid PVC, Antishock Injection Molding Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fittings for building trade
Physical Properties Metric English Comments
Density 1.35 - 1.39 g/cc
0.0488 - 0.0502 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Tensile Strength at Break 38.0 MPa
5510 psi
ISO R 527
Tensile Strength, Yield 44.0 MPa
6380 psi
ISO R527
Elongation at Break 130 %
130 %
ISO R 527
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Thermal Properties Metric English Comments
Vicat Softening Point 77.0 - 79.0 °C

@Load 5.00 kg
171 - 174 °F

@Load 11.0 lb
ISO R306
Users viewing this material also viewed the following: