Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fainplast Compounds PM 82/FR Flexible PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds PM 82/FR Flexible PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Pipes, UL 94 Class V0
Physical Properties Metric English Comments
Density 1.24 - 1.28 g/cc
0.0448 - 0.0462 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 79 - 83
79 - 83
ISO R 868
Tensile Strength at Break 18.0 MPa
2610 psi
ISO R 527
Elongation at Break 250 %
250 %
ISO R 527
Thermal Properties Metric English Comments
Brittleness Temperature -22.0 °C
-7.60 °F
Cold Flex; ISO 458/2
Flammability, UL94 V-0
V-0