Fainplast Compounds HGKA 87 Flexible PVC, Sheathing for High Temperatures Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds HGKA 87 Flexible PVC, Sheathing for High Temperatures Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Operating temperature 90°C
Physical Properties Metric English Comments
Density 1.35 - 1.39 g/cc
0.0488 - 0.0502 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Hardness, Shore A 85 - 89
85 - 89
ISO R 868
Tensile Strength at Break >= 15.0 MPa
>= 2180 psi
ISO R 527
Elongation at Break >= 300 %
>= 300 %
ISO R 527
Thermal Properties Metric English Comments
Oxygen Index 24 %
24 %
ISO 4589
Descriptive Properties Value Comments
Thermal Stability (minutes) 110
CEI 20-34/3-2