Fainplast Compounds GA 82 Flexible PVC, Flame Retardant Sheathing

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds GA 82 Flexible PVC, Flame Retardant Sheathing.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General purposes
Physical Properties Metric English Comments
Density 1.55 - 1.59 g/cc
0.0560 - 0.0574 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 80 - 84
80 - 84
ISO R 868
Tensile Strength at Break >= 14.0 MPa
>= 2030 psi
ISO R 527
Elongation at Break >= 250 %
>= 250 %
ISO R 527
Thermal Properties Metric English Comments
Oxygen Index 29 %
29 %
ISO 4589
Descriptive Properties Value Comments
Thermal Stability (minutes) 65
CEI 20-34/3-2