ExxonMobil SpectraSyn Ultra™ 150 High VI Polyalphaolefin (PAO) Fluid

Category Fluid , Lubricant , Polyalphaolefin (PAO)
Manufacturer Exxon Chemical
Trade Name SpectraSyn Ultra™
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF ExxonMobil SpectraSyn Ultra™ 150 High VI Polyalphaolefin (PAO) Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: SpectraSyn Ultra™ High VI Polyalphaolefin (PAO) have high viscosity indices, low pour points, low traction, good air release, and low foaming tendency. The extremely high viscosity indices translate into improved flow at low temperatures and increased elastohydrodynamic lubricant film thickness at high temperatures. SpectraSyn Ultra™ High VI PAO are frequently combines with other synthetic basestocks (e.g. SpectraSyn Ultra™ PAO, Exterex™ esters, and/or Synesstic™ alkylated naphthalene) to obtain optical viscometric properties. ExxonMobil’s SpectraSyn Ultra™ High VI PAO are particularly suited for applications that require improved wear protection. Appearance: Bright & ClearAvailability: Africa & Middle East, Asia Pacific, Central America, Europe, North America and South AmericaInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.850 g/cc
<br>@Temperature 15.6 °C
0.0307 lb/in³
<br>@Temperature 60.1 °F
ASTM D4052
Brookfield Viscosity 14860 cP
<br>@Temperature 32.0 °C
14860 cP
<br>@Temperature 89.6 °F
ASTM D2983
128000 cP
<br>@Temperature -4.00 °C
128000 cP
<br>@Temperature 24.8 °F
ASTM D2983
Viscosity Measurement 218
218
Index; ASTM D2270
Kinematic Viscosity 56 cSt
<br>@Temperature 140 °C
56 cSt
<br>@Temperature 284 °F
ASTM D445
18000 cSt
<br>@Temperature 0.000 °C
18000 cSt
<br>@Temperature 32.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 1500 cSt
1500 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 150 cSt
150 cSt
ASTM D445
Evaporation Loss 0.30 %
<br>@Temperature 150 °C,<br> Time 79200 sec
0.30 %
<br>@Temperature 302 °F,<br> Time 22.0 hour
ASTM D972
Thermal Properties Metric English Comments
Pour Point -32.8 °C
-27.0 °F
ASTM D5950/D97
Flash Point >= 265 °C
>= 509 °F
COC; ASTM D92
Optical Properties Metric English Comments
Refractive Index 1.4695
1.4695
ASTM D1218
Chemical Properties Metric English Comments
Acid Value <= 0.10
<= 0.10
[mg KOH/g]; ASTM D974 (mod)
Descriptive Properties Value Comments
Color <0.5
ASTM D1500
Composition Water
&lt;50 ppm, ASTM D6304 (mod)
Density Correction Factor 0.000511 (g/cc)/°C
ASTM D1250
Kauri-Butanol Value 3.3
ASTM D1133
Noack Volatility 0.004
ASTM D5800/DIN 51581