ExxonMobil 20 Exxon XD-3

Category Fluid , Lubricant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil 20 Exxon XD-3.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Exxon XD-3 20, 30, 40 and 50 are premium diesel engine oils blended from high quality base oils and a balanced additive system to meet or exceed the lubrication protection requirements of American diesel engine builders. They are specifically formulated using a versatile blend of ashless dispersants, metallic detergents, and inhibitor chemistry to control oxidation, wear, corrosion and rust. Exxon XD-3 Monogrades are especially suited for two-cycle applications.Diesel powered equipment from American manufacturers; On-highway light and heavy-duty trucking; Off-highway industries including: construction, mining, quarrying, and agriculture; Two-cycle applications
Physical Properties Metric English Comments
Density 0.890 g/cc

@Temperature 15.0 °C
0.0322 lb/in³

@Temperature 59.0 °F
ASTM D4052
Viscosity Measurement 98
98
Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 66 cSt
66 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 8.5 cSt
8.5 cSt
ASTM D445
Ash 0.80 %
0.80 %
Sulfated Ash, wt%; ASTM D874
Thermal Properties Metric English Comments
Pour Point -30.0 °C
-22.0 °F
ASTM D97
Flash Point 250 °C
482 °F
ASTM D92
Chemical Properties Metric English Comments
Total Base Number 7.3
7.3
mg KOH/g; ASTM D2896