Material Notes:
Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and are resistant to shearing and viscosity loss so that system efficiency is maintained and internal pump leakage is minimised at high operating temperatures and pressures. These high quality hydraulic oils with controlled low-temperature flow properties also provide maximised anti-wear protection for high pressure vane, piston and gear pumps. They provide long oil/filter life and optimum equipment protection reducing both maintenance costs and product disposal costs. They were developed in conjunction with the major OEMs to meet the stringent requirements of severe hydraulic systems using high pressure, high output pumps as well as handling the critical requirements of other hydraulic system components such as close clearance servo-valves and the high accuracy numerically controlled (NC) machine tools. Their multi-metal compatibility properties allow their use with system components employing various alloys in their designs. The DTE 10M Series Oils are formulated with high quality base oils and a carefully balanced super-stabilised additive system that helps neutralise the formation of corrosive materials. They are designed to work with systems operating under severe conditions where high levels of anti-wear and film strength protection are needed, yet they are formulated to work where non-anti-wear hydraulic oils are generally recommended.Hydraulic systems critical to deposit build-up such as sophisticated Numerically Controlled (NC) machines, particularly where close clearance servo-valves are used; Systems where cold start-up and high operating temperatures are typical; Where small amounts of water are unavoidable and this water could damage components; In systems containing gears and bearings; Systems requiring a high degree of load-carrying capability and anti-wear protection; Applications where thin oil-film corrosion protection is an asset such as systems where small amounts of water are unavoidable; Machines employing a wide range of components using various metallurgy
Physical Properties Metric English Comments
Density 0.879 g/cc

@Temperature 15.0 °C
0.0318 lb/in³

@Temperature 59.0 °F
ASTM D4052
Viscosity Measurement 0.50
0.50
Shear Stability, % Kinematic Viscosity Loss; CED L-14-A-93
141
141
Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 46 cSt
46 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 7.86 cSt
7.86 cSt
ASTM D445
Thermal Properties Metric English Comments
Pour Point -42.0 °C
-43.6 °F
ASTM D97
Flash Point 216 °C
421 °F
ASTM D92
Electrical Properties Metric English Comments
Dielectric Strength 40.0 kV/mm
1020 kV/in
ASTM D877
Descriptive Properties Value Comments
Copper Strip Corrosion 1B
3 hrs @ 100°C
Foam Sequence I, ASTM D912 20/0
Foam Sequence II, ASTM D893 20/0
Foam Sequence III, ASTM D893 20/0
FZG Gear Test, DIN 51534, Fail Stage 11
Rust Prevention, Synthetic Sea Water pass
ASTM D665B