Material Notes:
Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having high compressive and hydrostatic strengths. This yields a product able to withstand the high hydrostatic pressures experienced by today’s manned and unmanned subsea vehicles.The BZ Grade of material is specially engineered, high performance syntactics capable of operating within much of the Bathypelagic Zone (4,000 meters or 13,100 feet). Due to the nature of the syntactic constituent materials, the BZ Grade is available in a range of densities and strengths. The product is cast in block, sheet or rod form and has isotropic properties. It may be cut or machined to any size or shape to consistent buoyancy at depth. Each block is cast as a single unit, but may be cut to fit the application requirement. Blocks or trimmed parts may also be bonded together to form a larger structure.
Physical Properties Metric English Comments
Density 0.449 - 0.513 g/cc
0.0162 - 0.0185 lb/in³
Water Absorption <= 3.0 %

@Time 86400 sec
<= 3.0 %

@Time 24.0 hour
at depth
Mechanical Properties Metric English Comments
Compressive Strength 35.9 MPa
5200 psi
Compressive Modulus 1.65 GPa
240 ksi
Hydrostatic Design Basis 48.3 MPa
7000 psi
Hydrostatic Crush Strength
Descriptive Properties Value Comments
Service Depth (feet) 13600
Service Pressure (psi) 6000
Copyright © lookpolymers.com All Rights Reserved