Material Notes:
Syntactic foams are a combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having high compressive and hydrostatic strengths. This yields a product able to withstand the high hydrostatic pressures experienced by today’s manned and unmanned subsea vehicles.The HZ Grade of syntactic has been formulated to survive the deepest depths of the ocean. This class of syntactic will survive crush pressures greater than 20,000 psi making for safe operation in the Hadal Zone. These engineered products can provide up to 24 pounds of buoyancy per cubic foot at these depths. Each block is cast as a single unit, but may be cut to fit the application requirement. Blocks or trimmed parts may also be bonded together to form a larger structure.
Physical Properties Metric English Comments
Density 0.609 - 0.673 g/cc
0.0220 - 0.0243 lb/in³
Water Absorption <= 3.0 %

@Time 86400 sec
<= 3.0 %

@Time 24.0 hour
at depth
Mechanical Properties Metric English Comments
Compressive Strength 97.9 MPa
14200 psi
Compressive Modulus 2.76 GPa
400 ksi
Hydrostatic Design Basis 110 MPa
16000 psi
Hydrostatic Crush Strength
Descriptive Properties Value Comments
Service Depth (feet) 28400
Service Pressure (psi) 12500