Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Elisto THERMOSTAR® MD 150 Pattern material

Category Other Engineering Material
Manufacturer Elisto
Trade Name THERMOSTAR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elisto THERMOSTAR® MD 150 Pattern material.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Industrial laminateInformation provided by elisto
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
Water Absorption 0.20 %
0.20 %
Mechanical Properties Metric English Comments
Flexural Strength 150 MPa

@Temperature 23.0 °C
21800 psi

@Temperature 73.4 °F
Flexural Modulus 12.0 GPa
1740 ksi
Compressive Strength 300 MPa

@Temperature 23.0 °C
43500 psi

@Temperature 73.4 °F
Descriptive Properties Value Comments
Application Temperature (°C) 140
Users viewing this material also viewed the following: