Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman 811P Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman 811P Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Injection grade. With its high melt index, the material flows well in molding machines and fills large molds with ease. It is used for molding housewares and other items where a flexible, easy molding formula is desired. 811 natural as supplied by Eastman Chemical may lawfully be used in food contact (noncooking) subject to FDA 21 CFR 177.1520(c)(2.1).Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.916 g/cc
0.0331 lb/in³
ASTM D4883
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.00 MPa
1310 psi
500 mm/min (20 in./min.); Type IV Specimen; ASTM D638
Tensile Strength, Yield 9.00 MPa
1310 psi
500 mm/min (20 in./min.); Type IV Specimen; ASTM D638
Elongation at Break 300 %
300 %
500 mm/min (20 in./min.); Type IV Specimen; ASTM D638
Flexural Modulus 0.172 GPa
24.9 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Brittleness Temperature -45.0 °C
-49.0 °F
ASTM D746
Descriptive Properties Value Comments
Process Extrusion