Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EDRO #8 Premium 420 Stainless Mold Steel

Category Metal , Ferrous Metal , Stainless Steel , T 400 Series Stainless Steel
Manufacturer EDRO
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EDRO #8 Premium 420 Stainless Mold Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EDRO #8™ is a chromium-alloyed stainless tool steel with the following properties: excellent corrosion resistance, superior polishability, good wear resistance, good machinability, and stability in hardening. EDRO #8™ is recommended for all types of molding tools, its special properties make it particularly suitable for molds with the following demands: corrosion/staining resistance, i.e., for molding of corrosive materials, e.g. PVC, acetates, and for molds subjected to humid working/storage conditions; Wear resistance, i.e., for molding abrasive/filled materials, including injection-molded thermosetting grades - also for molds with exceptionally long production runs, e.g. electrical/electronic parts; disposable cutlery and containers; High surface finish, i.e., for production of optical parts, such as camera and sunglass lenses, and for medical containers, e.g. syringes, analysis phials.EDRO #8™ is resistant to corrosive attack by water, water vapor, weak organic acids, dilute solutions of nitrates, carbonates and other salts.Information provided by EDRO
Physical Properties Metric English Comments
Density 7.67 g/cc

@Temperature 399 °C
0.277 lb/in³

@Temperature 750 °F
Hardened and tempered to 50 HRC
7.75 g/cc

@Temperature 199 °C
0.280 lb/in³

@Temperature 390 °F
Hardened and tempered to 50 HRC
7.81 g/cc

@Temperature 20.0 °C
0.282 lb/in³

@Temperature 68.0 °F
Hardened and tempered to 50 HRC
Mechanical Properties Metric English Comments
Hardness, Brinell 215
215
Delivery condition (soft annealed)
Hardness, Rockwell C 38

@Treatment Temp. 566 °C
38

@Treatment Temp. 1050 °F
Tempered twice for 2 hr at temperature
50

@Treatment Temp. 482 °C
50

@Treatment Temp. 900 °F
Tempered twice for 2 hr at temperature
52

@Treatment Temp. 177 °C
52

@Treatment Temp. 350 °F
Tempered twice for 2 hr at temperature
53

@Treatment Temp. 260 °C
53

@Treatment Temp. 500 °F
Tempered twice for 2 hr at temperature
55

@Treatment Temp. 399 °C
55

@Treatment Temp. 750 °F
Tempered twice for 2 hr at temperature
55

@Treatment Temp. 93.3 °C
55

@Treatment Temp. 200 °F
Tempered twice for 2 hr at temperature
Tensile Strength, Ultimate 1420 MPa
206000 psi
45 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
1770 MPa
256000 psi
50 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
2070 MPa
300000 psi
55 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
Tensile Strength, Yield 1280 MPa
185000 psi
45 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
1470 MPa
213000 psi
50 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
1610 MPa
234000 psi
55 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
Elongation at Yield 8.0 %
8.0 %
in 2", 55 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
10 %
10 %
in 2", 50 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
12 %
12 %
in 2", 45 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
Reduction of Area 27 %
27 %
55 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
30 %
30 %
50 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
40 %
40 %
45 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
Modulus of Elasticity 190 GPa

@Temperature 399 °C
27500 ksi

@Temperature 750 °F
210 GPa

@Temperature 199 °C
30400 ksi

@Temperature 390 °F
214 GPa

@Temperature 20.0 °C
31100 ksi

@Temperature 68.0 °F
Izod Impact 16.3 J

@Treatment Temp. 510 °C
12.0 ft-lb

@Treatment Temp. 950 °F
Tempered for 2 hr
20.3 J

@Treatment Temp. 371 °C
15.0 ft-lb

@Treatment Temp. 700 °F
Tempered for 2 hr
20.3 J

@Treatment Temp. 149 °C
15.0 ft-lb

@Treatment Temp. 300 °F
Tempered for 2 hr
27.1 J

@Treatment Temp. 260 °C
20.0 ft-lb

@Treatment Temp. 500 °F
Tempered for 2 hr
32.5 J

@Treatment Temp. 649 °C
24.0 ft-lb

@Treatment Temp. 1200 °F
Tempered for 2 hr
74.6 J

@Treatment Temp. 760 °C
55.0 ft-lb

@Treatment Temp. 1400 °F
Tempered for 2 hr
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 20.0 - 199 °C
6.10 µin/in-°F

@Temperature 68.0 - 390 °F
11.5 µm/m-°C

@Temperature 20.0 - 399 °C
6.40 µin/in-°F

@Temperature 68.0 - 750 °F
Specific Heat Capacity 0.460 J/g-°C

@Temperature 20.0 °C
0.110 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 22.9 W/m-K

@Temperature 20.0 °C
159 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
23.9 W/m-K

@Temperature 199 °C
166 BTU-in/hr-ft²-°F

@Temperature 390 °F
24.9 W/m-K

@Temperature 399 °C
173 BTU-in/hr-ft²-°F

@Temperature 750 °F
Component Elements Properties Metric English Comments
Carbon, C 0.38 %
0.38 %
Chromium, Cr 13.6 %
13.6 %
Iron, Fe 84.42 %
84.42 %
As Balance
Manganese, Mn 0.50 %
0.50 %
Silicon, Si 0.80 %
0.80 %
Vanadium, V 0.30 %
0.30 %
Descriptive Properties Value Comments
Color Code Brown
Copyright © lookpolymers.com All Rights Reserved