E-Polymers EFLEX® I2010 Ionomer

Category Polymer , Thermoplastic , Ionomer
Manufacturer E-Polymers Co. Ltd.
Trade Name EFLEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers EFLEX® I2010 Ionomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
I-series (Ionomer): E-FLEX Ionomer is a family of ethylene acrylic acid (E/AA) copolymers, in which part of the acrylic acid is neutralized with metal ions such as zinc (Zn) or sodium (Na) or magnesium (Mg). E-FLEX Ionomer resins deliver impact toughness, abrasion resistance and chemical resistance in a variety of consumer and industrial products. E-FLEX Ionomer can be used in packaging, molded consumer goods, sports goods, and polymer modification.Information Provided by E-Polymers Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ASTM D792
Melt Flow 1.3 g/10 min
1.3 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 38.95 MPa
5649 psi
ASTM D882
Elongation at Break 350 %
350 %
ASTM D882
Descriptive Properties Value Comments
Metal Cation Na