Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dynasol Solprene® 1217 Solution Styrene-Butadiene Rubber (SSBR)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Dynasol
Trade Name Solprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dynasol Solprene® 1217 Solution Styrene-Butadiene Rubber (SSBR).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Solprene1217 is a linear random-block styrene/butadiene copolymer having 25% of styrene content, 17.5% present as a polystyrene block. It has a non-staining antioxidant system, BHT/TNPP free, FDA approved for use in food contact applications and is essentially gel free with a very clear color. It is available in bales wrapped in low melting point polyethylene.Uses: Solprene 1217 is used as compounding ingredient for adhesives, as modifier for thermoplastic resins. It is an excellent asphalt modifier or, for formulation of caulks and sealants; it is also an excellent processing aid for most polymers, giving good low temperature resistance. Used in extruded goods, soles, and heels.Applications: Plastic modificationInformation provided by Dynasol.
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
DIN 53479
Volatiles <= 0.75 %
<= 0.75 %
NM-300-01
Viscosity 4000 cP
4000 cP
30% Toluene; NM 300-18
Mooney Viscosity 47

@Temperature 100 °C
47

@Temperature 212 °F
ML (1+4); ASTM D1646
Chemical Properties Metric English Comments
Styrene Content 17.5 %
17.5 %
Block; NM 202-07
25 %
25 %
ASTM D5775
Descriptive Properties Value Comments
Color <15
Apha, NM 300-33
Insolubles 0.1
NM 300-15
Users viewing this material also viewed the following: