Category Fluid
Manufacturer Duratherm
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Duratherm FG Paraffinic Heat Transfer Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Duratherm FG - thermal oil rated to 620°F it is engineered and manufactured to comply with the demands of food grade applications. NSF registered, meets USDA requirements for incidental food contact (H1) and meets the requirements of 21CFR1783570. Information provided by Duratherm.
Physical Properties Metric English Comments
Density 0.678 g/cc
<br>@Temperature 288 °C
0.0245 lb/in³
<br>@Temperature 550 °F
0.705 g/cc
<br>@Temperature 316 °C
0.0255 lb/in³
<br>@Temperature 600 °F
0.731 g/cc
<br>@Temperature 260 °C
0.0264 lb/in³
<br>@Temperature 500 °F
0.732 g/cc
<br>@Temperature 204 °C
0.0264 lb/in³
<br>@Temperature 400 °F
0.843 g/cc
<br>@Temperature 37.8 °C
0.0304 lb/in³
<br>@Temperature 100 °F
Kinematic Viscosity 0.70 cSt
<br>@Temperature 260 °C
0.70 cSt
<br>@Temperature 500 °F
0.83 cSt
<br>@Temperature 260 °C
0.83 cSt
<br>@Temperature 500 °F
0.97 cSt
<br>@Temperature 260 °C
0.97 cSt
<br>@Temperature 500 °F
Kinematic Viscosity at 40°C (104°F) 33.1 cSt
33.1 cSt
Kinematic Viscosity at 100°C (212°F) 5.9 cSt
5.9 cSt
Molecular Weight 395 g/mol
395 g/mol
Average
Vapor Pressure 0.00482 bar
<br>@Temperature 204 °C
3.62 torr
<br>@Temperature 400 °F
0.0241 bar
<br>@Temperature 260 °C
18.1 torr
<br>@Temperature 500 °F
0.05723 bar
<br>@Temperature 288 °C
42.92 torr
<br>@Temperature 550 °F
0.10687 bar
<br>@Temperature 316 °C
80.157 torr
<br>@Temperature 600 °F
Thermal Properties Metric English Comments
Specific Heat Capacity 2.01 J/g-°C
<br>@Temperature 37.8 °C
0.480 BTU/lb-°F
<br>@Temperature 100 °F
2.51 J/g-°C
<br>@Temperature 204 °C
0.600 BTU/lb-°F
<br>@Temperature 400 °F
2.76 J/g-°C
<br>@Temperature 260 °C
0.660 BTU/lb-°F
<br>@Temperature 500 °F
2.80 J/g-°C
<br>@Temperature 288 °C
0.670 BTU/lb-°F
<br>@Temperature 550 °F
2.97 J/g-°C
<br>@Temperature 316 °C
0.710 BTU/lb-°F
<br>@Temperature 600 °F
Thermal Conductivity 0.130 W/m-K
<br>@Temperature 288 °C
0.900 BTU-in/hr-ft²-°F
<br>@Temperature 550 °F
0.131 W/m-K
<br>@Temperature 316 °C
0.912 BTU-in/hr-ft²-°F
<br>@Temperature 600 °F
0.133 W/m-K
<br>@Temperature 204 °C
0.924 BTU-in/hr-ft²-°F
<br>@Temperature 400 °F
0.135 W/m-K
<br>@Temperature 260 °C
0.936 BTU-in/hr-ft²-°F
<br>@Temperature 500 °F
0.1453 W/m-K
<br>@Temperature 37.8 °C
1.008 BTU-in/hr-ft²-°F
<br>@Temperature 100 °F
Pour Point -17.2 °C
1.00 °F
Flammability Test 466
466
Fire Point, °F
682
682
Autoignition Temp, °F
Flash Point 227 °C
440 °F
Descriptive Properties Value Comments
Distillation range at 10% 769
Distillation Range at 90% 930
Max Bulk Temp (°F) 620
Max Film Temp (°F) 670