Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dura-Bar G2A Continuously Cast Gray Iron Bar Stock ASTM A48

Category Metal , Ferrous Metal , Cast Iron , Alloy Cast Iron , Gray Cast Iron
Manufacturer Dura-Bar
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dura-Bar G2A Continuously Cast Gray Iron Bar Stock ASTM A48.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Dura-Bar G2A has Type D graphite in a predominantly pearlitic matrix. The fine graphite structure allows excellent surface finish and is normally used in permanent mold applications requiring optimal strengths and wear resistance. The microstructure will contain Type VII, type D, size 6-8, graphite as defined in ASTM A247. The matrix is predominantly pearlite. The rim will be similar to the center. Chill carbides will be less than 5% in any field at 100x and will be well dispersed. G2A Dura-Bar can be oil quench hardened from 1600F (870C) to a minimum hardness of 50 Rc on the outside of the bar. The inside diameter hardness will be less than 50 Rc. Lower quench hardnesses on the inside diameters are a result of larger graphite flakes and not a loss of matrix hardness.Composition: Typical chemical composition and ranges, actual values depend on cross section size.Information provided by Dura-Bar.
Mechanical Properties Metric English Comments
Hardness, Brinell 248 - 311
248 - 311
Tensile Strength, Ultimate 276 MPa
40000 psi
Shear Strength 207 MPa
30000 psi
Component Elements Properties Metric English Comments
Carbon, C 2.6 - 3.75 %
2.6 - 3.75 %
Manganese, Mn 0.20 - 0.40 %
0.20 - 0.40 %
Phosphorous, P <= 0.12 %
<= 0.12 %
Silicon, Si 2.0 - 3.0 %
2.0 - 3.0 %
Sulfur, S <= 0.02500 %
<= 0.02500 %
Descriptive Properties Value Comments
Endurance Ratio 0.5
Heat-Treat Response (Rc) 55-60
Relative Damping Capacity 250
Natural log of rate of successive amplitude.
Relative Wear Resistance Fair
Users viewing this material also viewed the following: