Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Teijin® Tetoron® HS Polyester Film, 500 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Teijin® Tetoron®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF DuPont Teijin Films Teijin® Tetoron® HS Polyester Film, 500 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Teijin® Tetoron® HS is a very clear polyester film. It is available in a wide range of thicknesses.Typical Applications: OHP SheetLabelsITOLaminated CardsWindow FilmInformation provided by DuPont.
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 200 %
200 %
ASTM D882A
Film Elongation at Break, TD 140 %
140 %
ASTM D882A
Coefficient of Friction, Dynamic 0.27
0.27
ASTM D1894
Coefficient of Friction, Static 0.30
0.30
ASTM D1894
Film Tensile Strength at Break, MD 195.9 MPa
28420 psi
ASTM D882A
Film Tensile Strength at Break, TD 227.9 MPa
33060 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 0.80 %

@Temperature 150 °C,
Time 1800 sec
0.80 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.10 %

@Temperature 150 °C,
Time 1800 sec
0.10 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Haze 2.3 %
2.3 %
ASTM D1003