Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 38.1 µm Thickness  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 38.1 µm Thickness  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile strength, puncture strength, elongation and heat seal strength compared to conventional films. Ideal for lamination to other substrates such as Dartek® nylon film or Mylar® polyester film for vacuum packaging applications. SL, in converter combinations, is particularly suited for the vacuum packaging of processed meats.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
Moisture Vapor Transmission 0.470 cc-mm/m²-24hr-atm
1.19 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
Water Vapor Transmission 12.4 g/m²/day
0.799 g/100 in²/day
ASTM E96 Procedure E
Oxygen Transmission 236 cc-mm/m²-24hr-atm
599 cc-mil/100 in²-24hr-atm
or 6200 cc/m²-24hr-atm for the film. ASTM D3985
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 600 %
600 %
ASTM D882
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D882
Dart Drop Test 100 g
0.221 lb
Seal Strength >= 1800 g/25 mm
>= 1800 g/in
Sentinel Sealer Test
Film Tensile Strength at Break, MD 34.0 MPa
4930 psi
ASTM D882
Optical Properties Metric English Comments
Haze 8.0 %
8.0 %
ASTM D1003
Gloss 100 %
100 %
20°; ASTM D2457