Material Notes:
PRIMACOR® 5980I dispersible polymer is an ethylene acrylic acid copolymer (20 wt % comonomer) which is dispersible in aqueous alkali and amines. Excellent adhesion to metallic, cellulosic, glass and other substrates are achievable. It also offers low heat seal temperature, high hot tack, excellent water, grease and oil resistance, high gloss, excellent clarity, low odor, and high wet strength retention. It is crosslinkable and is a versatile binder for nonwoven fibers including polypropylene, polyester, glass, and nylon etc. When used unmodified for food packaging applications, this resin complies with the U.S. Food, Drug and Cosmetic Act as amended under Food Additive Regulation 21 CFR 177.1310(c). The regulation should be consulted for complete details.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.958 g/cc
0.0346 lb/in³
Melt Flow 300 g/10 min

@Load 2.16 kg
300 g/10 min

@Load 4.76 lb
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
Tensile Strength, Ultimate 9.70 MPa
1410 psi
Elongation at Break 390 %
390 %
Modulus of Elasticity 0.0331 GPa
4.80 ksi
Molded Sample 2% Secant Modulus
Thermal Properties Metric English Comments
Vicat Softening Point 42.0 °C
108 °F