Dow Nordel® IP 4520 Molded Golf Grip

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Dow Chemical
Trade Name Nordel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Nordel® IP 4520 Molded Golf Grip.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FormulationNordel® IP 4520
Physical Properties Metric English Comments
Density 1.057 g/cc
0.03819 lb/in³
Mooney Viscosity 33

@Temperature 100 °C
33

@Temperature 212 °F
ML 1 + 4
Mechanical Properties Metric English Comments
Hardness, Shore A 58
58
Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 13.5 MPa
1960 psi
Vulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 685 %
685 %
Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 0.00160 GPa
0.232 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
200% Modulus 0.00270 GPa
0.392 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
300% Modulus 0.00380 GPa
0.551 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Tear Strength 29.5 kN/m
168 pli
Die C, Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 95 %

@Temperature 125 °C
95 %

@Temperature 257 °F
Pellets cured MDR TC95 + 15 min at 160°C, 70 hr at 125°C; Method B
Thermal Properties Metric English Comments
Brittleness Temperature -45.0 °C
-49.0 °F
Temperature Retraction, TR-10