Dow Corning SILASTIC® LS 4-9062 FLUOROSILICONE RUBBER

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® LS 4-9062 FLUOROSILICONE RUBBER.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
65 durometer, off-white, uncatalysed, fluorosilicone base.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc

@Temperature 25.0 °C
1.36 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Tensile Strength, Ultimate 7.10 MPa
1030 psi
Tensile Strength, Yield 2.50 MPa
362 psi
at 150% Elongation, maximum
Elongation at Break 311 %
311 %
Tear Strength 19.3 kN/m
110 pli
Compression Set 13 %
13 %
Processing Properties Metric English Comments
Shelf Life 36.0 Month
36.0 Month
Descriptive Properties Value Comments
Color off-white