Dow Corning 2-5573 Performance Modifier

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 2-5573 Performance Modifier.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Surface active silicone designed for reducing surface tension in silicone emulsions and improving drainage in pulp brownstock washing.Information provided by Dow Corning
Physical Properties Metric English Comments
Viscosity 4450 cP
4450 cP
Dynamic
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Active Content (%) 100
EO Content (%) 35
HLB Ratio (%) 6.3
Silicone HLB Content (%) 10.4