Material Notes:
Buna® SB 1712 - Schkopau is manufactured by cold polymerization using mixed rosin acid / fatty acid soaps. It is plasticized with 37.5 parts of an aromatic oil in relation to solid rubber. A discoloring stabilizer is added during the production process. Buna® SB 1712 - Schkopau is a general purpose rubber. It can be processed in all sectors of the tire and rubber industry. The main application is tire production. It is supplied in bales weighing 25 kg. Bales are wrapped in 50 micron PE film. At mixing temperatures above 115°C, the rubber can be processed with the packaging film. Information provided by Dow
Physical Properties Metric English Comments
Viscosity Measurement 2.2

@Temperature 160 °C
2.2

@Temperature 320 °F
[dNm]; ML, (0.5 RAD); ASTM D5289
3.0

@Temperature 160 °C
3.0

@Temperature 320 °F
[min]; ts1, (0.5 RAD); ASTM D5289
6.5

@Temperature 160 °C
6.5

@Temperature 320 °F
[min]; T50, (0.5 RAD); ASTM D5289
11.3

@Temperature 160 °C
11.3

@Temperature 320 °F
[min]; T90, (0.5 RAD); ASTM D5289
17

@Temperature 160 °C
17

@Temperature 320 °F
[dNm]; MH, (0.5 RAD); ASTM D5289
Mooney Viscosity 50

@Temperature 100 °C
50

@Temperature 212 °F
[MU]; ML 1+4, massed sample; ASTM D1646-99 (7.2.2)
Ash 0.10 %
0.10 %
ASTM D5667
Collected Volatile Condensable Material 0.20 %
0.20 %
ASTM D5668
Storage Temperature <= 30.0 °C
<= 86.0 °F
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 23.0 MPa
3340 psi
Die C (35 min / 145°C); ASTM D412
Tensile Strength, Yield 12.5 MPa

@Strain 300 %
1810 psi

@Strain 300 %
ASTM D412
Elongation at Break 500 %
500 %
ASTM D412
Chemical Properties Metric English Comments
Acid Value 4.9
4.9
% Organic Acid; ASTM D5775
Styrene Content 23.5 %
23.5 %
Bound Styrene; ASTM D5775
Processing Properties Metric English Comments
Shelf Life >= 12.0 Month
>= 12.0 Month
Descriptive Properties Value Comments
Accelerator (TBBS) wt% 1
ASTM 3185-1A
Carbon Black wt% 50
ASTM 3185-1A; IRB 7
Stearic Acid wt% 1
ASTM 3185-1A
Sulfur content, % 1.75
ASTM 3185-1A
Total Extractables % 32.5
ASTM D5774
Zinc Oxide wt% 3
ASTM 3185-1A