Denka VINYKON S210060 PVC, S grade for transparent extrusion molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Denka
Trade Name VINYKON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Denka VINYKON S210060 PVC, S grade for transparent extrusion molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding, etc.
Physical Properties Metric English Comments
Density 1.224 g/cc
0.04422 lb/in³
JIS-Z-8807
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
JIS-K-6301
Tensile Strength at Break 15.89 MPa
2305 psi
JIS-K-6723
Elongation at Break 360 %
360 %
JIS-K-6723
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -32.0 °C
-25.6 °F
JIS-K-6723
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
100%M, %, JIS-K-6723 0.82