Material Notes:
100% biodegradable and compostable thermoplastic. The compostable resin blend performs well compared to LDPE and is BPI certified compostable under ASTM D-6400. Xylomer™ is modified lignin, an abundant, natural byproduct of the paper manufacturing process, blended with other compostable polymers. The main benefit of using Xylomer™ technology is that Xylobag™ bags break down into humus in approximately 180 days once it has reached the natural environment, improving soil structure and leaving a cleaner environment. With government regulation restricting the use of harmful high-density polyethylene bags, the Xylobag™ provides retailers with a viable, cheap bag alternative. The Xylobag™ allows consumers to eliminate unsightly plastic litter from their communities.Information provided by Cyclewood Solutions.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 263 %
263 %
Film Elongation at Break, TD 382 %
382 %
Elmendorf Tear Strength MD 204 g
204 g
Elmendorf Tear Strength TD 706 g
706 g
Dart Drop Test 118 g
0.260 lb
Film Tensile Strength at Break, MD 14.36 MPa
2083 psi
Film Tensile Strength at Break, TD 10.85 MPa
1574 psi