Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.21 g/cc | 0.116 lb/in³ | ASTM C20 |
Water Absorption | 0.00 % | 0.00 % | ASTM 373 |
Particle Size | 3.0 - 10 µm | 3.0 - 10 µm | Thin Section Crystal Size |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Knoop Microhardness | 27 | 27 | 1000 g |
Modulus of Elasticity | 434 GPa | 62900 ksi | ASTM C848 |
Flexural Strength | 517 MPa | 75000 psi | ASTM F417 |
Poissons Ratio | 0.21 | 0.21 | ASTM C848 |
Fracture Toughness | 3.50 MPa-m½ | 3.19 ksi-in½ | Notched Beam |
Shear Modulus | 179 GPa | 26000 ksi | Calculated |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.60 µm/m-°C @Temperature 25.0 - 1000 °C |
2.56 µin/in-°F @Temperature 77.0 - 1830 °F |
ASTM C372 |
Specific Heat Capacity | 0.665 J/g-°C | 0.159 BTU/lb-°F | ASTM E1269 |
Thermal Conductivity | 115 W/m-K | 798 BTU-in/hr-ft²-°F | ASTM C408 |
Maximum Service Temperature, Air | 1600 °C | 2910 °F | No Load |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | <= 0.100 ohm-cm | <= 0.100 ohm-cm | ASTM D1829 |
Descriptive Properties | Value | Comments |
---|---|---|
Color | Black |