Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ConocoPhillips Hydroclear® 150 Circulating Oil

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name Hydroclear®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Hydroclear® 150 Circulating Oil.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Conoco Hydroclear Circulating Oil is a high-quality, rust-inhibited circulating oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Circulating Oil is specially formulated with proprietary additive chemistry and is recommended for use in a variety of bearing, mild-duty hydraulic and circulating oil applications which require a lubricant with rapid water separation, rust and corrosion protection and foam control. Hydroclear Circulating Oil is specifically formulated for use in backup roll bearings found in ferrous and nonferrous rolling mills, general-purpose bearing lubrication, circulating oil systems, “once through” oiling systems, seal oil applications and other similar end uses. Hydroclear Circulating Oil is available in ISO 150 and 320 viscosity grades.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Density 0.875 g/cc
0.0316 lb/in³
Viscosity Measurement 95
95
Viscosity Index
Saybolt Viscosity at 100°F 842 SUS
842 SUS
Saybolt Viscosity at 210°F 81 SUS
81 SUS
Kinematic Viscosity at 40°C (104°F) 160 cSt
160 cSt
Kinematic Viscosity at 100°C (212°F) 15.3 cSt
15.3 cSt
ASTM Color 3.0
3.0
Thermal Properties Metric English Comments
Pour Point -15.0 °C
5.00 °F
Flash Point 266 °C
510 °F
Descriptive Properties Value Comments
ASTM Rust A&B Pass
Emulsion Characteristics (40-40-0) 10 minutes
Foam Control (Sequence I,II,III) 0-0-0
Users viewing this material also viewed the following: