Colorite Polymers 7866 Non-Phthalate 66 Series Vinyl Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Colorite Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Colorite Polymers 7866 Non-Phthalate 66 Series Vinyl Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: The Colorite 66 series is a family of non-toxic PVC compounds developed specifically for those medical device, food, and infant care items for which the use of a citrate* based non-phthalate plasticizer is desirable. The Colorite 66 series is produced from raw materials that are sanctioned for use under Title XXI of the Code of Federal Regulations. This family of compounds can be molded or extruded, whichever is required. Colorite 66 compounds are available in a complete range of hardnesses from very soft to semi-rigid. They are also available in ethylene oxide and radiation sterilizable grades. As with all Colorite non-toxic compounds, complete traceability and lot identification of all raw materials and finished products are maintained.Information provided by Colorite Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
ASTM D2240
Tensile Strength, Ultimate 17.4 MPa
2530 psi
ASTM D638
Elongation at Break 395 %
395 %
ASTM D638
100% Modulus 0.00807 GPa
1.17 ksi
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -26.0 °C
-14.8 °F
ASTM D746