Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame retardance, low temperature, or chemical resistance, are all available. Formulations for exterior or interior use.Typical Applications: Clear General Purpose Molding and ExtrusionInformation provided by Colorite Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 66
66
10 sec; ASTM D2240
Tensile Strength, Ultimate 11.7 MPa
1700 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
100% Modulus 0.00517 GPa
0.750 ksi
ASTM D638