Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories SAL85 Special Alumina brick

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories SAL85 Special Alumina brick.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.95 g/cc
0.107 lb/in³
Porosity 18 %
18 %
Mechanical Properties Metric English Comments
Compressive Strength 78.5 MPa
11400 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 6.80 µm/m-°C

@Temperature 1000 °C
3.78 µin/in-°F

@Temperature 1830 °F
Shrinkage 0.00 %

@Temperature 1600 °C,
Time 7200 sec
0.00 %

@Temperature 2910 °F,
Time 2.00 hour
Component Elements Properties Metric English Comments
Al2O3 86 %
86 %
Fe2O3 0.60 %
0.60 %
Descriptive Properties Value Comments
Main Application Lime Kiln, Cement kiln, Various Rotary kiln, Reheating furnace, Soaking Pits, Various high-temp. furnace
Refractories Under Load(2kg/?,T2?) 1,700
Refractoriness (SK) 40
Users viewing this material also viewed the following: