Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.02 g/cc
<br>@Temperature 1000 °C,<br> Time 10800 sec
0.0730 lb/in³
<br>@Temperature 1830 °F,<br> Time 3.00 hour
2.05 g/cc
<br>@Temperature 110 °C,<br> Time 86400 sec
0.0741 lb/in³
<br>@Temperature 230 °F,<br> Time 24.0 hour
23.0 g/cc
<br>@Temperature 1500 °C,<br> Time 10800 sec
0.831 lb/in³
<br>@Temperature 2730 °F,<br> Time 3.00 hour
Porosity 19 %
<br>@Temperature 110 °C,<br> Time 86400 sec
19 %
<br>@Temperature 230 °F,<br> Time 24.0 hour
22.5 %
<br>@Temperature 1000 °C,<br> Time 10800 sec
22.5 %
<br>@Temperature 1830 °F,<br> Time 3.00 hour
23 %
<br>@Temperature 1500 °C,<br> Time 10800 sec
23 %
<br>@Temperature 2730 °F,<br> Time 3.00 hour
Mechanical Properties Metric English Comments
Modulus of Rupture 0.003924 GPa
<br>@Temperature 110 °C,<br> Time 86400 sec
0.5691 ksi
<br>@Temperature 230 °F,<br> Time 24.0 hour
0.0063765 GPa
<br>@Temperature 1000 °C,<br> Time 10800 sec
0.92485 ksi
<br>@Temperature 1830 °F,<br> Time 3.00 hour
0.01226 GPa
<br>@Temperature 1500 °C,<br> Time 10800 sec
1.779 ksi
<br>@Temperature 2730 °F,<br> Time 3.00 hour
Thermal Properties Metric English Comments
Shrinkage -0.800 %
<br>@Temperature 1500 °C,<br> Time 10800 sec
-0.800 %
<br>@Temperature 2730 °F,<br> Time 3.00 hour
-0.300 %
<br>@Temperature 1000 °C,<br> Time 10800 sec
-0.300 %
<br>@Temperature 1830 °F,<br> Time 3.00 hour
-0.0500 %
<br>@Temperature 110 °C,<br> Time 86400 sec
-0.0500 %
<br>@Temperature 230 °F,<br> Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 40 %
40 %
SiO2 53 %
53 %
Descriptive Properties Value Comments
Main Applications General furnace
Material Required for Estimating (kg/?) 2,050