China-Yixing Longly Refractories Alumina Plates and Pieces Microcrystal Wear-Resistant Alumina Ceramic Lining Plates and Pieces

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer China-Yixing Longly Refractories Co. Ltd
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China-Yixing Longly Refractories Alumina Plates and Pieces Microcrystal Wear-Resistant Alumina Ceramic Lining Plates and Pieces.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LONGLY's wear-resistant alumina ceramic lining plates and pieces are special alumina ceramics produced on the basis of Al2O3 by dry pressing with rare metal oxide as solvent, sintered under a high temperature of 1700°C. They could endure various wear resistant demands according to specific condition.Characteristics: With a Rockwell hardness of HRA80-90 (just inferior to diamond), its wear resistance is far superior to wear-resistant steel and stainless steel, which is 266 times that of manganese steel and 171.5 times that of high chromium cast iron. The bulk density is 3.6 g/cc, just a half of steel, which could reduce equipment load. These alumina ceramic lining plates or pieces can be stuck to the interior wall of the equipment by strong heat resistant adhesive.Applications: As for those mechanical equipment of heavy wearing used in conveying system for coal and materials, pulverizing system, ash and dust removing system of enterprises related to thermal power, steel, smelting, machinery, coal, mine, chemical, cement and port, different types of products could be chosen as per specific need.Information Provided by China Yixing Longly Refractories Co. Ltd
Physical Properties Metric English Comments
Bulk Density 3.50 - 3.60 g/cc
0.126 - 0.130 lb/in³
Water Absorption <= 0.020 %
<= 0.020 %
Mechanical Properties Metric English Comments
Hardness, Mohs 9.0
9.0
Compressive Strength 1700 - 2200 MPa
247000 - 319000 psi
Crushing Strength
Fracture Toughness 6.00 - 6.80 MPa-m½
5.46 - 6.19 ksi-in½
Component Elements Properties Metric English Comments
Al2O3 91 - 95.8 %
91 - 95.8 %
Fe2O3 0.20 - 0.25 %
0.20 - 0.25 %
Descriptive Properties Value Comments
Wear Loss (%) 0.10-0.15