China Tungsten ST1365 PM Antifriction Parts

Category Metal , Ferrous Metal
Manufacturer China Tungsten
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten ST1365 PM Antifriction Parts.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by China Tungsten
Physical Properties Metric English Comments
Density 6.20 - 6.60 g/cc
0.224 - 0.238 lb/in³
Component Elements Properties Metric English Comments
Carbon, C 0.25 - 0.26 %
0.25 - 0.26 %
combine carbon
<= 1.0 %
<= 1.0 %
total
Copper, Cu 2.0 - 5.0 %
2.0 - 5.0 %
Iron, Fe 79 - 82.75 %
79 - 82.75 %
Other <= 3.0 %
<= 3.0 %
Descriptive Properties Value Comments
Oil %, Min 12
Skin Hardness (HR) 70-120