3M Dyneon™ FC 2123 Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer 3M Dyneon™
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF 3M Dyneon™ FC 2123 Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Dyneon™ Fluoroelastomer FC 2123 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The “dry” ingredients should be blended before adding to the masticated gum. For best results, Dyneon FC 2123 should be banded on the mill several minutes prior to adding the blended dry ingredients. Once mixed, the compounded stocks have good scorch resistance and storage stability.Composition: di-polymer of vinylidene fluoride and hexafluoropropyleneLow viscosity version of FC 2144Process targets: injection and transfer molding, extrusion, bonding and calenderingProprietary incorporated cure technologyExcellent hot tear properties for molding articles with complex geometric profilesExcellent compression set resistance for molded goodsInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
Mooney Viscosity 25

@Temperature 121 °C
25

@Temperature 250 °F
ML1+10
Mechanical Properties Metric English Comments
Hardness, Shore A 71
71
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C; ASTM D2240
Tensile Strength at Break 16.2 MPa
2350 psi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Elongation at Break 270 %
270 %
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
100% Modulus 0.00365 GPa
0.530 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Compression Set 20 %
20 %
Aged 70 hours @ 200°C
Thermal Properties Metric English Comments
Transformation Temperature -18.0 °C
-0.400 °F
TR10; ASTM D1329
Component Elements Properties Metric English Comments
Fluorine, F 65.9 %
65.9 %
Descriptive Properties Value Comments
Color Opaque Off-White
MH, Maximum Torque 10.1 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 200°C
11.6 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ML, Minimum Torque 0.7 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 200°C
0.9 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
Solubility Ketones and Esters
t`50, Time to 50% cure 0.6 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 200°C
1.6 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
t`90 - Time to 90% cure 1.2 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 200°C
2.9 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ts2 - Time to 2 in-lb rise from min 0.5 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 200°C
1.3 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C