Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Drive Train Fluid HD, SAE 10W.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesChevron Drive Train Fluids HD are high performance lubricants designed for use in transmissions, final drives, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or Allison C4 requirements. They are manufactured using highly refined base oils, detergents, dispersants, oxidation and corrosion inhibitors, antiwear and extreme pressure agents, and a foam suppressant. Chevron Drive Train Fluids HD are designed for both newly developed and older model drive train components. They offer excellent friction retention, wear control, seal compatibility, oxidation stability, and viscosity stability. The frictional characteristics of the fluid are retained over the life of the lubricant. Components are protected from wear, even in severe service and under high loads. They protect precision parts against wear under high load conditions by controlling the formation of corrosion, varnish, and sludge. Chevron Drive Train Fluids HD are compatible with new and traditional seal and clutch materials.ApplicationsChevron Drive Train Fluids HD are recommended foruse in Caterpillar transmissions, final drives, wetbrakes, Allison Powershift transmissions, torque converters, and hydraulic systems requiring a fluid meeting Allison C4 or Caterpillar TO-4 or TO-2 requirements.Under normal ambient temperatures, hydraulic systems will use the SAE 10W viscosity grade. SAE 10W and 30 are recommended for mobile hydraulic systems where operating requirements are severe. Transmissions will use the SAE 30 viscosity grade. Chevron Drive Train Fluids HD are also recommended for heavy duty off highway automatic transmissions requiring an SAE 10W, 30, 50 or 60 fluid. Final drives will use the SAE 50 viscosity grade at normal temperatures and the SAE 60 at high ambient temperatures. Chevron Drive Train Fluids HD are not recommended for use in combined farm tractor hydraulic and transmission systems where low brake chatter is a requirement.
Physical Properties Metric English Comments
API Gravity 30.4 °
30.4 °
Viscosity 4200 cP

@Temperature -25.0 °C
4200 cP

@Temperature -13.0 °F
Cold Crank
Viscosity Measurement 101
101
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 196 SUS
196 SUS
Saybolt Viscosity at 210°F 46 SUS
46 SUS
Kinematic Viscosity at 40°C (104°F) 38 cSt
38 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
ASTM D445
Thermal Properties Metric English Comments
Pour Point -33.0 °C
-27.4 °F
ASTM D97
Flash Point 225 °C
437 °F
ASTM D92