Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name Delo®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Delo® 100 Motor Oil, SAE 30.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Chevron Delo 100 Motor Oils are high performance crankcase oils for diesel engines.They are manufactured using selected premium paraffinic base oils and detergent, dispersant, wear control, antioxidant, corrosion inhibitor, and foam suppressant additives.Chevron Delo 100 Motor Oils are formulated to:Reduce the formation of piston deposits and varnish resulting from high temperature operation and sludge typical of low engine temperature serviceProtect against wear, rust, and corrosionReduce oil thickening due to excellent high temperature oxidation stabilityMaintain clean engines for long trouble free lifeApplications:Chevron Delo 100 Motor Oils are recommended for use in two- and four-stroke diesel engines in farm machinery, construction equipment, marine, and other off-highway applications.Chevron Delo 100 Motor Oils utilize the latest technology to provide excellent performance in older engines using either normal, high or low sulfur diesel fuels.The SAE 20 and 30 grades can be used in powershift transmissions requiring Caterpillar TO-2 oils. These two grades can also be used in mobile hydraulic systems where excellent EP antiwear protection is needed.Chevron Delo 100 Motor Oilsmeet API Service Categories CF-2, CD-II (SAE 30, 40, 50) CF, CDComply with Detroit Diesel Corporation two-stroke engine recommendations, including the 0.85% ash maximum limit for Series 149 enginesChevron Delo 100 Motor Oils are authorized by USDA for use in federally inspected meat and poultry plants as H2 lubricants with no food contact.
Physical Properties Metric English Comments
API Gravity 29.4 °
29.4 °
Viscosity Measurement 99
99
Viscosity Index
Kinematic Viscosity at 40°C (104°F) 110 cSt
110 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 12.1 cSt
12.1 cSt
ASTM D445
Ash 0.76 %
0.76 %
Sulfated Ash wt%
Thermal Properties Metric English Comments
Pour Point -30.0 °C
-22.0 °F
ASTM D97
Flash Point 246 °C
475 °F
ASTM D92
Component Elements Properties Metric English Comments
Phosphorous, P 0.098 %
0.098 %
Zinc, Zn 0.108 %
0.108 %
Chemical Properties Metric English Comments
Total Base Number 7.0
7.0
ASTM D2896