Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Marlex® CL-200YB (Black) Rotational molding crosslinkable high density polyethylene  (discont

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Crosslinkable
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® CL-200YB (Black) Rotational molding crosslinkable high density polyethylene  (discont.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Benefits: crosslinks during molding - has outstanding melt strength at 204°C, is formulated to provide maximum UV protection for long-term outdoor weathering, contains an internal mold release, excellent stress cracking resistance to gasoline and other chemicals, outstanding impact strength at temperatures as low as -40°CCharacteristics: 95 J at 3 mm Impact Strength (-40°C); ARM Test Method, 260 J at 6 mm Impact Strength (-40°C); ARM Test MethodApplications: trash containers and lids for automated refuse collection systems, industrial and agricultural chemical storage tanks, small engine, snowmobile, and marine fuel tanks, tractor fuel tanksInformation provided by Chevron Phillips Chemical Company
Physical Properties Metric English Comments
Density 0.943 g/cc
0.0341 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 1000 hour

@Temperature 50.0 °C
>= 1000 hour

@Temperature 122 °F
Condition A; ASTM D 1693
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM D638 Type IV
Elongation at Break 450 %
450 %
ASTM D638 Type IV
Flexural Modulus 0.690 GPa
100 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 124 °C
255 °F
ASTM D1525
Brittleness Temperature <= -90.0 °C
<= -130 °F
ASTM D746
Processing Properties Metric English Comments
Processing Temperature 246 - 326 °C
475 - 619 °F
oven temperature for hot air machines 246-326°C, Marlex crosslinkable resins require special handling during processing