Chevron Phillips MarFlex® HHM TR-258 Low Density Linear Polyethylene, Blown Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name MarFlex®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Chevron Phillips MarFlex® HHM TR-258 Low Density Linear Polyethylene, Blown Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This LDLPE is tailored for applications that require:Good processabilityGood melt strengthGood drawdownGood strengthSatin finishGood MD & TD shrinkageGood contact clarity and lower gel contentTypical blown film applications include:Pallet shrinkHeavy duty bagsConsumer and institutional shrink filmGeneral purpose packagingThis grade does not contain process aid, slip or antiblock.Information provided by Chevron Phillips Chemical Company LP.
Physical Properties Metric English Comments
Specific Gravity 0.923 g/cc
0.923 g/cc
ASTM D1505
Melt Flow 0.20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 380 %
380 %
2.5 BUR; ASTM D882
460 %
460 %
4 BUR; ASTM D882
Film Elongation at Break, TD 650 %
650 %
4 BUR; ASTM D882
800 %
800 %
2.5 BUR; ASTM D882
Coefficient of Friction 0.35
0.35
2.5 BUR; ASTM D1894
0.35
0.35
4 BUR; ASTM D1894
Elmendorf Tear Strength, MD 0.472 g/micron
12.0 g/mil
2.5 BUR; ASTM D1922
1.18 g/micron
30.0 g/mil
4 BUR; ASTM D1922
Elmendorf Tear Strength, TD 15.7 g/micron
400 g/mil
4 BUR; ASTM D1922
37.2 g/micron
945 g/mil
2.5 BUR; ASTM D1922
Dart Drop 1.81 g/micron
46.0 g/mil
2.5 BUR; ASTM D1709
5.51 g/micron
140 g/mil
4 BUR; ASTM D1709
Film Tensile Strength at Break, MD 61.0 MPa
8850 psi
4 BUR; ASTM D882
72.0 MPa
10400 psi
2.5 BUR; ASTM D882
Film Tensile Strength at Break, TD 30.0 MPa
4350 psi
2.5 BUR; ASTM D882
46.0 MPa
6670 psi
4 BUR; ASTM D882
1% Secant Modulus, MD 365 MPa
52900 psi
2.5 BUR; ASTM D882
365 MPa
52900 psi
4 BUR; ASTM D882
1% Secant Modulus, TD 400 MPa
58000 psi
4 BUR; ASTM D882
500 MPa
72500 psi
2.5 BUR; ASTM D882
Optical Properties Metric English Comments
Haze 33 %
33 %
2.5 BUR; ASTM D1003
36 %
36 %
4 BUR; ASTM D1003
Gloss 40 %
40 %
at 60°, 4 BUR; ASTM D2457
46 %
46 %
at 60°, 2.5 BUR; ASTM D2457