Teknor Apex Beetle® PBTC115F Polybutylene Terephthalate and Polyethylene Terephthalate

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , PBT + PET Blend, Glass Filled , Polyethylene Terephthalate (PET)
Manufacturer Teknor Apex Company
Trade Name Beetle®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Beetle® PBTC115F Polybutylene Terephthalate and Polyethylene Terephthalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: PBTC115F is a 15% glass fiber reinforced PBT/PET alloy. It provides a good balance of mechanical performance and thermal endurance with excellent surface finish and mold release. Features: Good Mold Release; Good Thermal Stability; Good Surface Finish; High Gloss Processing Method: Injection Molding Forms: Pellets Injection Notes: Drying is necessary if material has been exposed to air for longer than 3 hours; Back Pressure: Low; Injection Pressure; High; Injection Rate: Moderate Resin ID (ISO 1043): PBT+PET-GF 15Information Provided by Teknor Apex
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Processing Properties Metric English Comments
Rear Barrel Temperature 250 - 280 °C
482 - 536 °F
Middle Barrel Temperature 250 - 280 °C
482 - 536 °F
Front Barrel Temperature 250 - 280 °C
482 - 536 °F
Melt Temperature <= 260 °C
<= 500 °F
Processing Temperature
Mold Temperature 130 - 150 °C
266 - 302 °F
Drying Temperature 120 °C
248 °F
Dry Time 4 hour
4 hour
Screw Speed 50 - 100 rpm
50 - 100 rpm