Chengdu Polyster PET Film PET Films/Sheets

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Chengdu Polyster Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster PET Film PET Films/Sheets.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High transparency, is specially manufactured for thermoforming products and printing products. It is suitable for the packaging of foods, cosmetics, medicines and other products, and it is also used for printing plastic cards and stationaries, etc.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Thickness 4.44 - 30.5 microns
0.175 - 1.20 mil
Storage Temperature 23.0 - 30.0 °C
73.4 - 86.0 °F
Descriptive Properties Value Comments
Optimum Storage Humidity (%) 70