Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CeramTec MZ BE Zirconia 3Y-TZP, Dental Grade

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer CeramTec North America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CeramTec MZ BE Zirconia 3Y-TZP, Dental Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MZ BE is a yttria-stabilized tetragonal zirconia used in dental applications.
Physical Properties Metric English Comments
Density 6.04 g/cc
0.218 lb/in³
without HIP; DIN EN 623-2
Particle Size 0.40 µm
0.40 µm
Grain
Weibull Modulus 15
15
DIN ENV 843-5
Mechanical Properties Metric English Comments
Vickers Microhardness 1250
1250
HV 0.5; DIN ENV 843-4
Tensile Modulus 214 GPa
31000 ksi
Young's; DIN ENV 843-2
Flexural Strength 1100 MPa
160000 psi
Bending Strength; 4-Point without HIP; DIN ENV 843-1
Poissons Ratio 0.30
0.30
DIN ENV 843-2
Fracture Toughness 5.00 MPa-m½
4.55 ksi-in½
SEVNB; ISO 23 146
Shear Modulus 82.3 GPa
11900 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 20.0 - 600 °C
6.11 µin/in-°F

@Temperature 68.0 - 1110 °F
DIN EN 821-1
Component Elements Properties Metric English Comments
Al2O3 0.25 %
0.25 %
DIN ISO 12677
HfO2 1.9 %
1.9 %
DIN ISO 12677
Y2O3 5.4 %
5.4 %
DIN ISO 12677
ZrO2 92.4 %
92.4 %
DIN ISO 12677
Descriptive Properties Value Comments
Color White
Monoclinic Content (%) < 1
DIN ISO 12677