C.O.I.M. FILCO® 658 N Non Ionic Aqueous Emulsion of Unsaturated Polyester Polymer

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer C.O.I.M. S.p.A.
Trade Name FILCO®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF C.O.I.M. FILCO® 658 N Non Ionic Aqueous Emulsion of Unsaturated Polyester Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Non Ionic Aqueous Emulsion of Unsaturated Polyester PolymerGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are collectively known as FILCO®. The products in the FILCO® line serve to size glass fiber, to optimize the mechanical characteristics of the fiber, or to bind the fibers for the production of mat.Applications: Filco 658 N has been studied as an insoluble binder for glass fiber. Particularly for chopped strand mat, continuous strand mat and perform.It is also suggested as a film forming component of glass fiber sizing for SMC, BMC, and DMC.When Filco 658 N is used as an insoluble liquid binder benzoyl peroxide must be added (0.6 - 1.2% of active peroxide on Filco 658 N). Temperatures between 160°C and 190°C for 40 - 60 seconds are recommended for the binder cross link in the dryers during the mat production process.When Filco 658 N is used as a film former in glass fiber sizing formulations for SMC, BMC, and DMC no benzoyl peroxide should be added.In both applications the resulting products make thermosetting glass/resin composites having good physical and mechanical properties. Information provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Solids Content 48 - 52 %
48 - 52 %
Particle Size 0.60 - 1.0 µm
0.60 - 1.0 µm
MA147LFE
pH 1.5 - 2.5
1.5 - 2.5
MA148LFE
Brookfield Viscosity 1.2 - 2.2 cP

@Temperature 20.0 °C
1.2 - 2.2 cP

@Temperature 68.0 °F
Brookfield RVT spindle 2.2 RPM
Descriptive Properties Value Comments
Appearance Milky Liquid
Copyright © lookpolymers.com All Rights Reserved