Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CIMBAR BARIMITE™ XF High Purity Barite (BaSO4)

Category Ceramic , Other Engineering Material , Additive/Filler for Polymer
Manufacturer CIMBAR Performance Minerals
Trade Name BARIMITE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CIMBAR BARIMITE™ XF High Purity Barite (BaSO4).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Barimite Products are natural, off-white barites produced in Cartersville, Georgia. Cimbar's broad range of Barimite products are clean, high purity, high specific gravity, low solubility and chemically inert. These properties have made Barimite products the industry standard for consistent quality and performance in a wide range of end-use applications.Uses:Coatings: Automotive Primers, Automotive Topcoats, High Gloss Enamel, Powder Coatings, Semi-gloss Latexes, Gloss Latexes, Industrial Coatings, Architectural CoatingsFillers: Plastics, Ceramics, Friction Materials, Rubber, Plastisols, Adhesives, Latex Products, Urethane Foams, Acoustical Compounds, Insulating Materials, Sound Attenuation ProductsInformation provided by Cimbar Performance Minerals.
Physical Properties Metric English Comments
Specific Gravity 4.39 g/cc
4.39 g/cc
Oil Absorption 12 %
12 %
Fineness 6.0
6.0
Hegman Fineness
Apparent Bulk Density 1.20 g/cc
0.0434 lb/in³
Loose
1.84 g/cc
0.0666 lb/in³
Compacted
Moisture Absorption at Equilibrium 0.10 %
0.10 %
Loss On Ignition 0.30 %
0.30 %
Particle Size 2.5 µm
2.5 µm
Median
<= 15 µm
<= 15 µm
Max
Particle Mesh Size 325 Mesh
325 Mesh
0.0% retained
pH 8.0
8.0
Component Elements Properties Metric English Comments
Al2O3 0.060 %
0.060 %
Fe2O3 0.20 %
0.20 %
SiO2 0.50 %
0.50 %
Trace Metals 0.040 %
0.040 %
Heavy Metals
Descriptive Properties Value Comments
BaSO4 (%) 96