Material Notes:
Recovered polyethylene compositeInformation provided by Breplast S.p.A.
Physical Properties Metric English Comments
Melt Flow 2.0 - 3.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 - 3.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Descriptive Properties Value Comments
Color Light
Users viewing this material also viewed the following: