Bostik 6384 General Purpose Characteristics EVA Glue Stick

Category Polymer , Adhesive , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer Bostik
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Bostik 6384 General Purpose Characteristics EVA Glue Stick.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Bostik 6384 General Purpose Characteristics EVA Glue StickGeneral purpose characteristics. Bonds plastics, wood, porous materials.
Physical Properties Metric English Comments
Viscosity 18000 cP

@Temperature 177 °C
18000 cP

@Temperature 350 °F
Typical
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 51.7 °C
125 °F
Minimum Service Temperature, Air -28.9 °C
-20.0 °F
Processing Properties Metric English Comments
Pot Life 0.67 min
0.67 min
Open Time
Descriptive Properties Value Comments
Color Translucent