Borealis Borseal™ TD110BF Terpolymer for BOPP Film

Category Polymer , Film , Thermoplastic
Manufacturer Borealis
Trade Name Borseal™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borseal™ TD110BF Terpolymer for BOPP Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Borseal TD110BF is a C2/C4 terapolymer film resin.Borseal TD110BF is especially developed for use as sealing layers in coextruded BOPP film (manufactured on Stenter frame and double bubble film processes).Information provided by the Manufacturer.
Physical Properties Metric English Comments
Melt Flow 6.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Flexural Modulus 0.700 GPa
102 ksi
ISO 178
Heat Seal Strength Initiation Temperature 103 °C
217 °F
3 N; Borealis Test
Thermal Properties Metric English Comments
Melting Point 128 - 132 °C
262 - 270 °F
ISO 3146
Vicat Softening Point 114 °C
237 °F
10 N; ISO 306
Optical Properties Metric English Comments
Haze 1.8 %
1.8 %
ASTM D1003