Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Beijing Evergrow Resources ER-WR-40G Polypropylene Super-Fine Filter Material

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Beijing Evergrow Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Evergrow Resources ER-WR-40G Polypropylene Super-Fine Filter Material.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Use: bag filter, etc.Information provided by Beijing Evergrow Resources.
Descriptive Properties Value Comments
Air Resistance (Pa) <16
0.32L/min-cm²
<8
0.06L/min-cm²
Efficiency (%) >85
0.32L/min-cm²
>95
0.06L/min-cm²
European Standard F7
Weight (g/m²) 37-43
Width (mm) <=1000
Users viewing this material also viewed the following: