Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bapolene® 213B Polyethylene, Extrusion Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Bapolene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 213B Polyethylene, Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Bapolene 213B is a low density polyethylene for molding, extrusion and foaming applications. It contains slip and complies with US FDA regulation 21 CFR 177.1520 (Olefin polymers), paragraph (c)2.1.Applications: General purpose foaming, extrusion, and molding.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
ASTM D-1505
Melt Flow 2.0 g/10 min
2.0 g/10 min
ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
Tensile Strength, Yield 10.17 MPa
1475 psi
ASTM D-638
Elongation at Break 700 %
700 %
>700; ASTM D-638
Flexural Modulus, 1% Secant 212 MPa
30700 psi
ASTM D-790
Descriptive Properties Value Comments
Process Extrusion
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: