| Category | Polymer , Thermoset , Polyurethane, TS | 
| Manufacturer | BCC Products | 
| Trade Name | |
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | BCC Products BC 8405 Urethane Casting.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792-66 | 
| Brookfield Viscosity | 190 cP | 190 cP | Mixed | 
| 480 cP | 480 cP | Part B | |
|           64           cP           @Temperature 23.9 °C  | 
                  64           cP           @Temperature 75.0 °F  | 
        Part A | |
| Linear Mold Shrinkage | 0.0010 cm/cm | 0.0010 in/in | ASTM D2566 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Shore D |           72 - 78                     @Temperature 23.9 °C  | 
                  72 - 78                     @Temperature 75.0 °F  | 
        ASTM D2240 | 
| Tensile Strength, Ultimate | 37.24 MPa | 5401 psi | ASTM D638 | 
| Elongation at Break | 11.6 % | 11.6 % | ASTM D638 | 
| Flexural Strength | 62.13 MPa | 9011 psi | ASTM D790 | 
| Flexural Modulus | 1.8264 GPa | 264.89 ksi | ASTM D790 | 
| Izod Impact, Notched | 0.705 J/cm | 1.32 ft-lb/in | ASTM D256 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Heat Distortion Temperature | 60.6 °C | 141 °F | ASTM D648 | 
| Processing Properties | Metric | English | Comments | 
|---|---|---|---|
| Cure Time |           120 - 240           min           @Temperature 25.0 °C  | 
                  2.00 - 4.00           hour           @Temperature 77.0 °F  | 
        demold time | 
| Pot Life |           15           min           @Temperature 25.0 °C  | 
                  15           min           @Temperature 77.0 °F  | 
        gel time, 200g; ASTM 2471-71 | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Mix Ratio | 1:1 by weight or volume |