Material Notes:
Formula: C3H6NNaO2CAS: 4316-73-8Description: Sarcosine Sodium 40% sol. is a colorless to yellowish liquid, with no odor. It is miscible with water in all proportions.Synonyms: N-Methylglycine monosodium salt, Sarcosine Sodium Salt, Sodium (methylamino) acetate, Sodium N-methylglycinateApplications: Intermediate used in the production of Pharmaceuticals, Industrial Chemicals, Textiles and Industry; Also used as a Initial Product for Chemical Synthesis and Corrosion inhibitorInformation provided by BASF
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
Molecular Weight 111.1 g/mol
111.1 g/mol
Thermal Properties Metric English Comments
Melting Point 1.00 - 10.0 °C
33.8 - 50.0 °F
Boiling Point 100 °C
212 °F
Descriptive Properties Value Comments
Assay 39.5 - 40.5%
Color <100
APHA, DIN EN 1557